Taklon vs PBT vs Nylon: Which Fiber for Your Makeup Brushes?
Taklon vs PBT vs Nylon comes down to three labels and two polymers. Taklon is a trade name for tapered filament, usually polyester; PBT is the polyester polymer commonly used for it; nylon is a polyamide with about 11 times the commercial moisture regain. Specify polymer, diameter and taper.
Key takeaways
- Taklon vs PBT is a naming question. Taklon is a trade name for tapered filament, and PBT, polybutylene terephthalate, is the polyester polymer commonly used to make it. Nylon is a polyamide, a different polymer.
- ASTM D1909 lists a commercial moisture regain of 0.4% for polyester and 4.5% for nylon. These are defined trade values, so a nylon head still has to be checked wet and dry.
- A published tapering process for PBT uses alkaline hydrolysis, for example 30% sodium hydroxide at about 60°C for 6–12 hours. Taper is a processing step, which is why tapered taklon costs more than standard PBT.
- On our cost table, standard-diameter PBT is the 1.0× baseline and fine tapered taklon sits at 1.4–2.0×. The spec that holds a bulk order names polymer, diameter in millimeters, tip treatment, blend ratio and tuft density.
Taklon vs PBT vs Nylon: three labels, two polymers
Taklon vs PBT vs Nylon is often presented as a comparison of three synthetic makeup brush fiber types. It is not. Taklon is a trade name, PBT is a polymer and nylon is a polymer family. Once the three names are separated, the fiber line on a specification becomes short to write.
- Taklon names a trade grade: tapered synthetic filament, in practice usually polyester. Our taklon option spans 0.06–0.10 mm, and the name alone does not fix the polymer, the diameter inside that range or the length of the taper.
- PBT, polybutylene terephthalate, names a thermoplastic polyester. It says nothing about diameter, or about whether the tip is tapered or cut level.
- Nylon names a polyamide family that includes nylon 6, 66 and 612. Its tip can be level, tapered or flagged.
Brush-filament maker Stucchi traces how the names arose. Nylon was the first synthetic paintbrush filament, developed by DuPont in the 1950s, mechanically tapered and then flagged. For cosmetic brushes, Stucchi describes that filament as too stiff and lacking fine tips.
The change came in the 1970s, when DuPont found a way to chemically taper polyester and sold the patent to Toray Industries. Toray developed the process with Japanese brush makers, among them Takamoto, which used its Taklon brand. The patent expired in the 1990s and other companies began production. Stucchi's history also notes PBT as the usual polymer for artist-grade filament, with PET used for standard grades and priced considerably lower.
Why PBT is the polyester that tapers
Natural hair narrows to a fine tip. A synthetic filament cut straight across ends in a flat edge, and that edge is what reads as scratchy. Tapering is the step that turns level filament into something that can stand in for hair, and PBT takes that step well.
Publication WO 2013/008609 lists PBT and PET as its polyester options and nylon 6, 66 and 612 as its polyamide options. It prefers PBT because the polymer dissolves quickly and forms a taper with a constant gradient. The example process holds the filament tip in 30% sodium hydroxide at about 60°C for 6–12 hours, so the surface dissolves toward a point.
US patent 4,381,325, granted to Toray Industries in 1983, names PBT or its copolymers as the most preferable polyester for hair-like tapered fibers. It also records that alkali treatment renders the fiber surface hydrophilic and leaves fine variation on that surface.
Two cautions follow. The conditions above describe published processes, not a universal recipe, and other routes such as bicomponent spinning exist. Nylon can be tapered as well, but the same publication lists a phenol-based solvent for polyamide in place of the alkaline bath used on polyester. Polymer and taper route are separate lines on a specification.
Nylon: the polyamide with higher moisture regain
Nylon is a polyamide, and its amide groups hold water. The trade table reflects that. ASTM D1909-13(2026) lists a commercial moisture regain of 4.5% for nylon and 0.4% for polyester, which puts nylon at about 11 times polyester. The standard is explicit that these are defined values for calculating commercial weight, not measured results for a given lot, and that actual regain depends on the material's history.
For a brush buyer the useful consequence is a test, not a ranking. A nylon head can feel different wet from dry and can take longer to release water after washing. Compare each sample in both states, and time how long the head takes to dry after a standard wash.
In our supplier attribute records, nylon is named as the brush material on 2 SKUs, one for eye use and one for cheek use. Nylon is therefore not confined to detail tools, and each of those SKUs still needs its own diameter and taper written down.
How the fiber choice changes with the formula
Diameter and taper decide most of what the customer feels, and the polymer sets the starting point. The ranges below are the ones used on this site: 0.06–0.07 mm as the mainstream vegan standard, 0.04–0.05 mm for sensitive-skin and finishing brushes, and 0.08–0.10 mm for firm buffing and detail work. The fiber grades guide covers the diameter bands in full.
| Formula or task | Fiber to specify | What to check on the sample |
|---|---|---|
| Liquid and cream foundation, concealer | Tapered PBT or taklon, 0.06–0.07 mm | Even release without streaking |
| Loose and pressed powder | Tapered PBT, 0.06 mm, or a natural-hair option | Pickup and diffusion |
| Brow, liner and lash detail | Nylon or firm PBT, 0.08–0.10 mm | Spring and tip recovery after bending |
| Sensitive skin and finishing | Tapered PBT, 0.04–0.05 mm | Tip fineness under magnification |
PBT appears in every row; nylon appears in one. The vegan and natural hair comparison explains why synthetic is the default for liquid, cream and powder alike, and why natural hair now survives on heritage positioning rather than performance.
What the price difference actually pays for
On our cost table, standard-diameter PBT is the 1.0× baseline and fine tapered taklon sits at 1.4–2.0×. That gap is not a polymer premium. Chemical tapering dissolves material in a controlled bath and narrows the tip, and a finer diameter needs more filaments to fill the same tuft. The private label cost guide breaks the finished brush down block by block.
Diameter moves the number as well. There is a 2× price difference between 0.05 mm and 0.08 mm taklon. PET is the cheaper polyester in Stucchi's account, so a low quote for "taklon" can mean a PET filament, a level tip or a coarser diameter rather than the tapered PBT in the sample.
Ask for the three values in writing: polymer, diameter in millimeters and tip treatment. A golden sample and a fiber lot number turn that line into something the bulk order can be checked against.
One way to see what those values look like when they are published is the face brush listings, where fiber appears as a spec line rather than a marketing adjective, and a blank entry means the factory never confirmed it in writing.
The fiber spec that holds a bulk order
Five fields make the fiber enforceable: polymer, diameter in millimeters, tip treatment, blend ratio and tuft density. A workable line reads "PBT, 0.07 mm, chemically tapered", followed by the blend and tuft weight for that SKU. The tech pack guide shows where each field sits on the sheet. Add the fiber lot number to the batch record so a later order can be traced to the same filament.
Run 3 checks on the sample before approval. Look at the tips under magnification and confirm a taper rather than a flat cut. Bend the head and watch whether the filaments return. Wash the sample and repeat the bend test, because nylon and polyester respond differently to moisture.
If fibers come loose during the wash test, use the shedding guide, since loose fibers left from cutting and an anchoring failure have different causes. The sample evaluation guide gives the nine physical tests for the finished brush.
Frequently asked questions
Is taklon the same as PBT?
Not quite. Taklon is a trade name for tapered synthetic filament, usually polyester. PBT is the polyester polymer commonly used to make it. The name alone does not show whether the filament is PBT, PET or a blend, so the specification should name the polymer, diameter and taper rather than the trade name.
Which is softer, taklon or nylon?
Softness is set mainly by diameter and tip. A 0.04–0.05 mm tapered polyester reads softer than a 0.08 mm level nylon. Compare samples at the same diameter and taper instead of ranking the polymers by name.
Is nylon good for makeup brushes?
Yes, for tasks that need spring and control, such as brow, liner and lash work. Nylon is a polyamide with higher moisture regain than polyester, so check the head wet, dry and after washing. In our supplier attribute records, nylon is named on an eye brush and a cheek brush.
Is taklon fiber suitable for a vegan makeup brush?
Taklon is synthetic and contains no animal hair, so the filament suits a vegan claim. The claim still depends on every other component. Adhesive, handle finish and any PU case must also be animal-free, which the <a href="/resources/product-and-technical/vegan-vs-natural-hair-makeup-brushes">vegan claim guide</a> covers component by component.
Why does tapered fiber cost more than level fiber?
Tapering is an added process. A published PBT method holds the filament tip in alkaline solution, for example 30% sodium hydroxide at about 60°C for 6–12 hours, to dissolve it toward a point. On our cost table that places fine tapered taklon at 1.4–2.0× against the 1.0× baseline for standard-diameter PBT.
How do I write the fiber line in a tech pack?
Name five fields: polymer, diameter in millimeters, tip treatment, blend ratio and tuft density. For example: PBT, 0.07 mm, chemically tapered, single diameter, with tuft weight in grams per SKU. Add the fiber lot number to the batch record and keep a golden sample from the approved lot.
Can a supplier swap nylon for PBT without re-sampling?
No. The polymers differ in moisture regain, and the taper route can differ as well. A swap can change how the head feels wet, how it dries and how it returns after bending, so treat any polymer change as a new sample rather than a like-for-like substitution.